当前位置 -> 首页新闻资讯无锡环氧地坪漆的脱落原因与防范技巧 发布时间:(2019/9/14)

无锡环氧地坪漆的脱落原因与防范技巧

标签:混凝土密封固化剂 | 混凝土密封固化剂厂家

一般在环氧地坪漆施工后的一段时间有些施工后的无锡环氧地坪漆涂膜会产生与基层之间的附着力出现问题,其会使涂层小片脱离或者是与地面的整体脱离。出现这样的现象往往是环氧地坪漆厂家在环氧地坪漆施工时有许多因素没注意造成的。

Generally, after the construction of epoxy floor paint for a period of time, some of the epoxy floor paint film after construction will produce adhesion problems with the base layer, which will make the coating patches or the overall separation from the ground. This phenomenon is often caused by many factors neglected by epoxy floor paint manufacturers in the construction of epoxy floor paint. 其主要原因有以下:

The main reasons are as follows:


1、在施工前进行场内预处理不当,地面还有其余杂质如油污,水溶解物,锈迹等,施工环境清理不干净。

1. The improper pretreatment before construction and other impurities on the ground, such as oil, water soluble substances, rust, etc., make the construction environment unclean.


2、其中一个在预处理时到环氧地坪漆施工时的间隔时间过长,导致灰尘杂质继续出现在地表面。

2. The interval between pretreatment and epoxy floor paint construction is too long, which leads to dust impurities continuing to appear on the surface.


3、还有就是在处理时地面的没有干好就开始进行施工操作。需知如果在潮湿的地面上进行施工,就会有环氧地坪漆层脱离地面的风险存在。

3. There is also the construction operation that starts when the ground is not well done. It is necessary to know that if construction is carried out on wet ground, there will be a risk that the epoxy floor paint layer will break away from the ground.


4、地面材料基底与环氧地坪漆涂层结合不理想,原因是由于基地材料光滑程度比较高,不易与其附着,这其中也可能是环氧环氧地坪漆的涂料配置不适当,这需要根据当地环境因素来进行配置。

4. The combination of the base material and the epoxy floor paint coating is not ideal. The reason is that the base material is not easy to adhere to because of its high smoothness. It may also be that the coating configuration of the epoxy floor paint is inappropriate, which needs to be configured according to local environmental factors.


5、没有对地面层做烘干处理,或者烘干处理不足,导致环氧环氧地坪漆厂家在进行环氧地坪漆施工时出现涂层不稳定脱落的现象。

5. There is no drying treatment for the surface layer or insufficient drying treatment, which results in unstable peeling of the epoxy floor paint during the construction of the epoxy floor paint by the epoxy floor paint manufacturer.


防范措施:

Preventive measures:


1、环氧地坪漆厂家对即将进行施工的环氧地坪进行表面的清理,如遇到光滑程度较高的地面则用喷砂,或用砂质对其进行处理,使其粗糙度增强,方便施工。

1. The epoxy floor paint manufacturer cleans the surface of the epoxy floor which is going to be constructed. If it encounters the surface with higher smoothness, it will be treated with sand blasting or sand, so as to enhance its roughness and facilitate construction.


2、在处理好等地面风干不能过长,一般都是3-4个小时左右,就要开始施工。也可以同时对地面进行干燥处理。

2. The ground air-drying can not be too long when it is well handled. Generally, it takes about 3-4 hours to start construction. The ground can also be dried at the same time.


3、地坪漆厂家在无锡环氧地坪漆施工时要选择好与其基层地质适合度高的材料,要保证其附着力能够适应其地面的材质。

3. Floor paint manufacturers should choose materials with high geological suitability with their base when constructing epoxy floor paint, and ensure that their adhesion can adapt to the material of their floor.

本站网址:http://www.wuxispeed.com


来源:无锡环氧地坪公司  浏览次数:993
相关阅读:如何保证无锡环氧地坪施工质量的五个关键点 | 分析客户对无锡环氧地坪施工中应注意的问题 | 无锡环氧地坪冬季施工注意及施工前的考虑因素
 
 
产品分类    
普通型环氧地坪 环氧玻璃钢(FRP)地坪 丙烯酸地坪
环氧砂浆地坪 乙烯基酯重防腐地坪 EPPU聚合型工业地坪
环氧彩砂地坪 非金属金属耐磨地坪 停车场地坪
环氧自流平地坪 混凝土密封固化剂 环保型无毒防霉墙面
环氧防静电地坪 自流平水泥地坪 有机硅丙烯酸室外防腐地坪


联系我们
电 话:0510-88706248/13915319875
传 真:0510-88706348
邮 箱:Yxdspeed@163.com
网 址:www.wuxispeed.com
地 址:无锡市东亭锡沪东路11号
版权所有:无锡市思必德科技有限公司    网站关键词:无锡环氧地坪  混凝土密封固化剂  苏ICP备20046775号    技术支持:无锡易商科技    网站地图
友情链接:梳理机 台州讨债公司 合肥讨债公司 金华讨债公司 盐城环氧地坪 合肥停息挂账 无锡保洁公司 脚手架厂家 无锡环氧地坪